I have seen the same error in our facility. It's something very soft ,
black color and it can be very long and thin. The location is always under
the conductor of the laminate.
I have seen the problem in two laminates suppliers and in thin (0,25 mm)
and thick (1,6 mm) FR4 material.
I think that the spots are in the treated side of the cooper foil,but I'm
not sure.
Xavier Angel LAB CIRCUITS,S.A.
[log in to unmask]
----------
> De: Eltek Ltd. - Process Engineering <[log in to unmask]>
> A: [log in to unmask]
> Asunto: [TN] High resistance internal shorts
> Fecha: martes 5 de mayo de 1998 9:04
>
> Hi Technetters !
> During the past period we made a lot of improvements in our production to
> reduce the scrap due to internal shorts . At this moment 90% of internal
> shorts are " isolation shorts " , it mean high resisitivity .
> Some of this shorts were located and we found unidentificed spots in the
> laminates . The spots are located under the conductors ( laminate side )
,
> they have irregular shapes and are very thin . Such spots are bridging
two
> adjacent conductors . Such spots are not result of unetched copper since
> they are running deep into the laminate ( more than 25 microns ) .
> I will appreciate comments on this problem via technet or to my private
e-mail .
> Best regards
>
>
> Edward Szpruch
> Eltek Ltd - Israel
> Tel 972 3 9395050
> Fax 972 3 9309581
> E-mail : [log in to unmask]
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
> For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
> ################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|