TECHNET Archives

May 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
"Eltek Ltd. - Process Engineering" <[log in to unmask]>
Date:
Tue, 5 May 1998 10:04:16 +0300
Content-Type:
text/plain; charset="us-ascii"
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Eltek Ltd. - Process Engineering" <[log in to unmask]>
Parts/Attachments:
text/plain (31 lines)
Hi Technetters !
During the past period we made a lot of improvements in our production to
reduce the scrap due to internal shorts .  At this moment 90% of internal
shorts are " isolation shorts " , it mean high resisitivity .
Some of this shorts were located and we found  unidentificed spots in the
laminates . The spots are located under the conductors ( laminate side ) ,
they  have irregular shapes and are very thin . Such spots are bridging two
adjacent conductors . Such spots are not result of unetched copper since
they are running deep into the laminate ( more than 25 microns ) .
I will appreciate comments on this problem via technet or to my private e-mail .
Best regards


Edward Szpruch
Eltek Ltd - Israel
Tel  972 3 9395050
Fax 972 3 9309581
E-mail :  [log in to unmask]

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################


ATOM RSS1 RSS2