Fred,
although I am working for a PTFE/woven glass fabric manufacturer, I can tell you that based on many years of
experience in manufacturing FR4, BT/Epoxy, Polyimide, PTFE, etc. base materials, 400 MHz is still a good
frequency for FR4 - depending on tolerances.
Some design engineers use FR4 up to more than 1 GHz, whereas other ones use PTFE/woven glass laminates from
even as low as 200 MHz on.
Regards
Manfred Huschka
Taconic
--- On Thu, 21 May 1998 08:25:09 -0700 Fred Watt <[log in to unmask]> wrote:
Has anybody had any problems with FR-4 at 100 to 200 MHz? I have several boards from several
fabrication shops in which the signal loses amplitude above 80-100 MHz. The boards are controlled impedance
(50 Ohms) with 5 mil traces and 5 mil dielectrics. The traces are about 6.5" long.
I would appreciate any comments on this subject. The supplier of the material says that FR-4 should
be good to 400 MHz.
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
---------------End of Original Message-----------------
--------------------------------------------------------
Name: Manfred Huschka
Taconic Advanced Dielectric Division, Lynn Industrial Park, Mullingar,
Co. Westmeath, Republic of Ireland
Office: PF 1275, D-51676 Wipperfuerth, Germany
Tel.: +49 2267 888004
Fax: +49 2267 888005
E-mail: Manfred Huschka <[log in to unmask]>
Web: www.taconic-add.com
Date: 05/22/98
Time: 18:17:36
This message was sent by Z-Mail Pro - from NetManage
NetManage - delivers Standards Based IntraNet Solutions
--------------------------------------------------------
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|