Paul,
Normally you would use a self-shimming material for this type of application. Self-shimming simply means that microballoons [i.e. tiny glass or phenolic spheres, either hollow or solid} of a minimum diameter are added to the adhesive. When the adhesive bondline is squeezed down, the microballoons hold the two substrates apart by approximately the distance of the sphere diameter. 5 mil microballoons will give you consistent 5 mil bondlines. You could also use a glass scrim cloth, but I doubt your customer would go for that ...
Sheila @ tracor
----------
From: Paul Allen[SMTP:[log in to unmask]]
Sent: Tuesday, May 19, 1998 2:29 PM
To: [log in to unmask]
Subject: [TN] TN Electrical Conductive expoxy use of
Dear Tech Netters,
I have an application requiring the use of AIT electrical conductive
expoxy, ME 8452 does anyone have an experience in controlling thickness
of bond lines.Currently with our application bonding two PCB's together,
squeeze out is proving hard to control. Our customer wants zero. Any
ideas.
Paul Allan.
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|