TECHNET Archives

May 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Content-Type:
text/plain; charset=US-ASCII
X-To:
Paul Klasek <[log in to unmask]>
Date:
Wed, 20 May 1998 17:09:08 +0800
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Edwin C. Salido" <[log in to unmask]>
Subject:
From:
"Edwin C. Salido" <[log in to unmask]>
Content-Transfer-Encoding:
7bit
Sender:
Parts/Attachments:
text/plain (96 lines)
     Dear Paul,

        Nice to hear from you again. Before, we try to do something with
     syringe having air bubblesor gaps. If gap is near the tip, we squeeze
     out paste to remove. If it's in the middle , we tap the syringe
     against the table. This procedure is  not fool proof. But today and
     due to the criticality of 0402, we are returning syringe with air
     gaps.



     Rgds.,

     Edwin


______________________________ Reply Separator _________________________________
Subject: RE: [TN] Getting rid of Air Bubbles in Solder Paste Syringes
Author:  Paul Klasek <[log in to unmask]> at #SMTP
Date:    20/05/1998 01:56 PM


Hi Matthias
I am surprised you put up with the bubbles .
We return them as non conforming to specs., and that is the end of it .
With copy of A black mark in black book on top of it .
As you guessed correctly, without vacuum you can do very little ;
even than the bubbles can push the paste out of syringe ;
you really do not want to get into desperate modes like this .

Your syringes are capped on point with a pin pushing into exit ?
If they have just a screw on cap as most do ( standard EFD tip caps ) ,
that is one way to get the air in .
No fun to bubble on o805's , agree .

Sorry ; no tricks .
I'll forward you contact on Ed Salido ; Philips ; Manila ;
he may know better , doing o402's .

See you                     paul ; ResMed


>----------
>From:  Matthias Mansfeld[SMTP:[log in to unmask]]
>Sent:  Wednesday, 20 May 1998 8:19
>To:    [log in to unmask]
>Subject:       [TN] Getting rid of Air Bubbles in Solder Paste Syringes
>
>Hello Technetters,
>
>I have some solder paste syringes which contain air bubble, probably
>from transport. That means, I have to fight with a bit of overflow
>during dispensing, rather boring with 0805 or SOICs. Pull back flow
>is not so easy to set up with my equipment, thus, the best would be
>to get rid of these bubbles.
>Does anybody know an easy, proven trick? ( I have no vacuum chamber
>available).
>
>Many thanx in advance, regards
>Matthias Mansfeld
>-----------------------------------------------
>Matthias Mansfeld Elektronik
>* Printed Circuit Board Design and Assembly
>Am Langhoelzl 11, D-85540 Haar, GERMANY
>Phone: +49-89-4620 0937, Fax: +49-89-4620 0938
>E-Mail: [log in to unmask]
>Internet: http://home.t-online.de/home/matthias.mansfeld
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
>text in the body:
>To subscribe:   SUBSCRIBE TechNet <your full name>
>To unsubscribe:   SIGNOFF TechNet
>################################################################
>Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
>information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
>847-509-9700 ext.312
>################################################################
>
>

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2