I am experiencing solderability problems due to my oven glue procurement at
the wave solder. My pads are nice and shiny before the oven then they come
out with a haze that can't be wiped off or cleaned off with alcohol. Is
there anything that I am missing that could be caused by the oven? Would
nitrogen help this?
################################################################