Sender: |
|
Subject: |
|
From: |
|
Date: |
Fri, 15 May 1998 09:14:26 -0600 |
Reply-To: |
|
Parts/Attachments: |
|
|
Try Emerson & Cuming Stycast 1265. It is a two part clear epoxy, and it
adheres very well to glass, as long as the glass is clean. For technical
data, call Emerson & Cuming Specialty Polymers at 1-800-832-4929.
Heidi Jones
Senior Manufacturing Engineer
Honeywell, Defense Avionics Systems
9201 San Mateo NE
Albuquerque, NM 87113-2227
(505) 828-5806
FAX (505) 828-5500
email: [log in to unmask]
----------
From: Jean Connick[SMTP:[log in to unmask]]
Sent: Thursday, May 14, 1998 6:01 PM
To: [log in to unmask]
Subject: [TN] Help
Can anyone help me locate an Epoxy, RTV or other, that when cured is
semi rigid, with an excellent bond strength to glass. (A one part system
is preferred).
Thanks for any/all your assistance ahead of time
Jean Connick
Tel: 714-996-1248 x 299
Fax: 714-961-7836
E-Mail: [log in to unmask]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|