TECHNET Archives

May 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
TOSTEVIN_BC <[log in to unmask]>
Date:
Fri, 15 May 1998 08:04:16 -0400
X-To:
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, TOSTEVIN_BC <[log in to unmask]>
Parts/Attachments:
text/plain (64 lines)
     Only a true chemist would tell the rest of us to etch our windshields
     with a, "simple 10% solution of ammonium biflouride."  I must remember
     to ask for it at the auto parts store!

     Rudy, there's $$$ to be made in marketing a mirror adhesive kit that
     really works.  I'm - 0 for 10 - on those things.

     Bruce Tostevin
     Benchmark Electronics
     Hudson, NH


______________________________ Reply Separator _________________________________
Subject: Re: [TN] Help
Author:  RSedlak <[log in to unmask]> at 0UTG0ING
Date:    5/14/98 10:45 PM


Jean:

This is one of those experiences that may be exactly what you need, or may
also result in gales of laughter.

I had a similar need, to glue my rear view mirror to my windshield, in a non-
standard position.   I solved the problem by using standard Dow RTV silicone,
BUT, in order to get it to adhere, I had to roughen the surface of the glass,
using emery paper.

Now, using emery paper on your parts may be difficult, or impractical, and so
my suggestion is use a mild glass etch, which could be a simple 10% solution
of ammonium biflouride, which you could put on with a cotton swab.   Rinse
well, then dry, and apply your silicone.

Hope it works for you.

Rudy Sedlak
RD Chemical Company

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text
in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################


ATOM RSS1 RSS2