Yikees! Electroless Ni/ immersion gold is not compatible with soldered
BGA's? We need more than luck!
The only Proceedings listing I see on the IPC web page and in their
Publications 98 is was released in June 97. Do you have a document
number or other source for these 'allegations'?
Cheers,
Greg
-----Original Message-----
From: Josh Moody [SMTP:[log in to unmask]]
Sent: Wednesday, May 13, 1998 3:34 PM
To: [log in to unmask]
Subject: Re: [TN] Reliability of Immersion Gold PCB
If you would like a paper look into the proceedings
that occurred last Sept at IPC Surface Finish Summit in St.
Paul,MN.
There was a paper presented there that discusses the issues
behind electroless Ni/ immersion gold and why it is not
compatible
with soldered BGA's.
Good luck,
At 01:30 PM 5/13/98 -0400, you wrote:
>Hi Steve, thank you for your comment! What I really want to
know is the
>reliability of the product by using immersion gold PCB,
including solder
>joint reliablity and integrity of the PCB after process. Do you
know whether
>IPC has any standard or publication on this topic? Is it
Bellcore compliant?
>What is the issue with BGA for immersion gold?
>
>Thanks again!
>
>Fulton Feng
>
>> ----------
>> From:
>>
"STEVE_O\\'HARA"@HP-Vancouver-om10.om.hp.com[SMTP:"STEVE_O\\'HARA"@HP-Va
nc
>> ouver-om10.om.hp.com]
>> Sent: Wednesday, May 13, 1998 10:01 AM
>> To: Feng, Fulton [MPK:5221:EXCH]
>> Cc: [log in to unmask]
>> Subject: Re: [TN] Reliability of Immersion Gold PCB
>>
>> What do you want to know??
>>
>> Raw Board Reliability (solderability)
>> Contact Resistance Reliability?
>> Solder Joint Reliability
>>
>> With regards to Solder Joint Reliability, the solder
interface of the
>>
>> nickel to solder forms tin intermetallics which will not
be as strong
>>
>> as solder to solder. These joints will still be
acceptable for most
>> smt components but immersion gold and BGA's should be
avoided.
>>
>> Regards:
>>
>> Steve O'Hara HP
>>
>>
>> ______________________________ Reply Separator
>> _________________________________
>> Subject: [TN] Reliability of Immersion Gold PCB
>> Author: Non-HP-Fulton.Feng.ffeng ([log in to unmask])
at
>> HP-Vancouver,mimegw10
>> Date: 5/12/98 5:39 PM
>>
>>
>> Hi
>> Has anyboy done any reliability study on Gold Immersion PCB
finish?
>>
>> Thanks
>> Fulton Feng
>>
>>
################################################################
>> TechNet E-Mail Forum provided as a free service by IPC using
LISTSERV 1.8c
>>
>>
################################################################
>> To subscribe/unsubscribe, send a message to [log in to unmask]
with
>> following text
>> in the body:
>> To subscribe: SUBSCRIBE TechNet <your full name>
>> To unsubscribe: SIGNOFF TechNet
>>
################################################################
>> Please visit IPC web site (http://jefry.ipc.org/forum.htm)
for additional
>> inform
>> ation.
>> For the technical support contact Dmitriy Sklyar at
[log in to unmask] or
>> 847-509-97
>> 00 ext.311
>>
################################################################
>>
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using
LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask]
with
following text in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC web site (http://jefry.ipc.org/forum.htm) for
additional
information.
>For the technical support contact Dmitriy Sklyar at
[log in to unmask] or
847-509-9700 ext.311
>################################################################
>
>
Josh Moody
Materials Quality Engineer
Hewlett-Packard - Richardson (HPSD)
ph# (972) 497-4617
[log in to unmask]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using
LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask]
with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for
additional information.
For the technical support contact Dmitriy Sklyar at
[log in to unmask] or 847-509-9700 ext.311
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|