Phil Crepeau:
- If this is up for a vote, I vote with Werner and those folks who feel that
"the bigger the blob the better the job" does not apply to SMT.
- My vote is based on the results of an Air Force Manufacturing Technology
Study some years ago. If I recall correctly, that showed that larger
connections lasted longer only because the rate of crack propagation through
solder is fairly consistent, therefore it takes a larger volume of solder
longer to "fail" because it takes the crack more time to severe the
connection. The study found a solder connection with smaller solder volume
tended to last longer before cracks occurred and therefore were/are considered
more reliable. I have taken a quick look and cannot find a direct reference
to the study in my files. You might check with the MANTECH Information Office
at Wright Labs., Wright Patterson AFB where I think most of the AF MANTECH
tests are archived.
- Just my .02 worth. Jim Moffitt
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|