Solder samples are for:
1.- To check solderability of your boards.
2.- Solder samples are the rejects of your PCB Supplier.
3.- Are useful for show and tell samples, to run reflow oven profiles, to
check SMT placements with double side adhesive tape (if pads are good),
etc.
Mauricio Castro
______________________________ Reply Separator _________________________________
Subject: [TN] Solder Sample: Why, what to do, any IPC guide line?
Author: Ken Patel <[log in to unmask]> at INTERNET
Date: 08/5/98 9:39 AM
Hi all,
We receive solder sample with every lot. Can anyone tell me the what should
we do with that? Does our assembly house has any added value for us? Does
IPC has any guideline for solder sample?
Happy Friday to all off you.
re,
ken patel
______________________________________________________
Ken Patel Phone: (408) 490-6804
1708 McCarthy Blvd. Fax: (408) 490-6859
Milpitas, CA 95035 Beeper: (888) 769-1808
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text
in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|