Chris,
Please describe this solution. Is the nitric acid used as a rack
stripping solution or a specific compound such as "Copper (II)
nitrate, Hexahydrate" Cu(NO3)2*H2O ?
______________________________ Reply Separator _________________________________
Subject: [TN] Crashing copper
Author: "TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask] at
corp
Date: 5/7/98 9:26 AM
I have a question about copper. I have a solution of copper nitrate and I
want to crash all of the copper out of this solution. How would I go about
doing this?
Chris Coon
Borden Chemical
Kent, WA
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text
in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|