For what it is worth, the Gore SPEEDBOARD prepreg materials (epoxy and cyanate
ester) are very compatible with Rogers 4003, 4350 etc as well as FR-4 and
might be considered as the bonding sheets for those multilayer designs that
need a lower dielectric constant or thinner PWBs for controlled impedance
layers or higher signal speeds.
################################################################