Dear Mr. Lwalling
I would appreciate if you can tell me where we can get details of the Gore
SPEEDBOARD prepreg materials. Do they have a web site or can u give us their
mailing address or FAX for correspondence.
We are a design bureau in India always looking for this information. Any
help would be appreciated.
Regards
Murthy S.L.N.
Managing Director
ECAD Technologies Pvt.Ltd.
373/1a, Eleventh Cross, Seventh Main,
Second block, Jayanagar
Bangalore 560 011
INDIA
FAX 91 80 663 0738
PH: 91 80 663 2779
80 64179
email: [log in to unmask]
-----Original Message-----
From: Lwallig <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Date: 01 May 1998 23:46
Subject: Re: [DC] FR4 material/Rogers material compatibility?
>For what it is worth, the Gore SPEEDBOARD prepreg materials (epoxy and
cyanate
>ester) are very compatible with Rogers 4003, 4350 etc as well as FR-4 and
>might be considered as the bonding sheets for those multilayer designs that
>need a lower dielectric constant or thinner PWBs for controlled impedance
>layers or higher signal speeds.
>
>################################################################
>DesignerCouncil E-Mail Forum provided as a free service by IPC using
LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
>To subscribe: SUBSCRIBE DesignerCouncil <your full name>
>To unsubscribe: SIGNOFF DesignerCouncil
>################################################################
>Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
>For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
>################################################################
>
>
################################################################
DesignerCouncil E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE DesignerCouncil <your full name>
To unsubscribe: SIGNOFF DesignerCouncil
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|