Good morning,
I have a question regarding porosity testing. Can IPC Test method 2.3.24
be used for testing porosity of immersion gold over nickel, or is the
thickness of the gold to thin to withstand any porosity testing.
You can answer me on line or off line. My E-mail address is
[log in to unmask]
ph# 1-619-695-2222, ext. 243
fax 1-619-695-2165
Thank you,
Ron Hayashi
################################################################