Tennyson,

You'll either have to do a series of stress levels and then convert the
set of responses to an empirical equation that predicts the changing
response, or just test the stress level that's appropriate to the final
application. Be careful that the test method doesn't generate a creep
mechanism that differs from field service.

Andy Magee
Mechanical Engineer, Materials Engineer and Metallurgist.
[log in to unmask]

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################


ATOM RSS1 RSS2