Hi Technetters,
I have got this minor puzzle. If a material does not have a linear
visco-elastic region, are there any guidelines as to what stress to
apply for a creep test?
Tennyson
Tennyson Nguty, AeroMech Department, Newton Building, Salford University
Manchester M5 4WT, UK. Tel: 0161-295 5951/4696, Fax: 0161-295 5575/5108
################################################################