Another option is to use ionized air or Nitrogen to blow off contamination
from non-conductive materials. This has the added benefit of reducing the
static charge which will help to reduce further contamination.
To see ionization guns for clean rooms visit
http://www.electrostatics.com/ionizinggun.htm
At 04:33 PM 21-04-98 -0400, Phil Dam wrote:
>We use tack cloths to wipe down SS separator and lamination plates after
>cleaning (plate scraping) to remove debris, etc. We also use them as needed
>to clean up around our lay-up station for multilayers.
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
>For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
>################################################################
>
Peter Mariani
Ph. 215-513-0850
Fx. 215-513-0855
mailto:[log in to unmask]
Visit http://www.electrostatics.com
to learn more about static electricity
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################