1. Mil-F-14256 on fluxes was cancelled, and the IPC's J-STD-004 was adopted for
fluxes. All fluxes can be characterized per this document. J-STD-004 is called out
as the material specification in IPC's soldering standard J-STD-001. I am not
familiar with Def Stan 34-4 so I can't comment on this one.
2. EMPF in Indianapolis did some significant work proving that companies could
successfully use low residue fluxes and subsequently conformal coat. Specifications
are being changed to make these allowances.
3. Can't help on this one.
Dave
--------------------------------------------------------------------
David W. Bergman CAE
Vice President of Technical Programs
IPC
2215 Sanders Road
Northbrook, IL 60062-6135
P 847-509-9700 x340
F 847-509-9798
email [log in to unmask]
IPC's website www.ipc.org
--------------------------------------------------------------------
>>> Chris Evans <[log in to unmask]> 04/14/98 07:30PM >>>
Hello Technetters
I have three questions
1. Which specification are no clean fluxes released to. Do they
conform to Def Stan 34-4.? ( I know its not been issued other than in
draft form but it gets called up in our work)
2. Has anyone any information on conformal coating over no-clean flux.
Compatability or long term reliability issues ?
3. How are others going to overcome the new restrictions on rosin flux
fume ? Are you using extraction or changing fluxes ??
Any response greatfully received
Thanks
Chris Evans
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700
ext.311
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|