I hope these data would help you.
|-----------+-----------+-----------+-----------+-----------+-----------|
| | | | yarn | | |
|-----------+-----------+-----------+-----------+-----------+-----------|
|glass style|yarns/ inch| warp | fill | thickness | Oz/Yd |
| | | | | |(superscrip|
| | | | | | t: 2) |
|-----------+-----------+-----------+-----------+-----------+-----------|
| 2165 | 60 X 52 | E225 1/0 | G150 1/0 | 0.0040" | 3.55 |
|-----------+-----------+-----------+-----------+-----------+-----------|
| 7629 | 44 X 34 | G75 1/0 | G75 1/0 | 0.0071" | 6.19 |
|-----------+-----------+-----------+-----------+-----------+-----------|
################################################################