Hi Patrick,
The following site may give you some ideas for wave soldering optimisation:
http://www.swpc.co.il
Ducas,Patrick wrote:
> Good morning,
>
> I'm in the way to participate in a brainstorming session in order to
> optimize the wave soldering process (reduction of defects). We have the
> Soltec Delta machine and we use soluble fluxes in the process. I'm not
> related to this process but I have been requested to participate.
>
> I will greatly appreciate any suggestion, idea or trick from all of you
> regarding wave soldering process optimisation.
>
> Thanks for taking your time.
>
> Patrick
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
> For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
> ################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|