TECHNET Archives

April 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Ed Holton <[log in to unmask]>
Date:
Thu, 23 Apr 1998 11:39:49 -0400
Content-type:
text/plain; charset=US-ASCII
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (27 lines)
Looking for information about using a reducing atmosphere (or forming gas)
of nitrogen and hydrogen when soldering.  I just learned about this during
some related research.  In this application, a die is soldered to a
terminal using an 88%Pb solder preform (reflow 300C)  The comment was made
that this application could be done without flux by using a reducing
atmosphere of nitrogen and hydrogen, where at the high temperature (350C)
the hydrogen will "clean" the surface.  I am interested in any information
on this subject.

Thank You

Ed Holton
Hella Electronics
734-414-0994

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################


ATOM RSS1 RSS2