Alan,
I don't have the reference to hand here, but I think it was Roger Wild
(of IBM) that published some very strong evidence for life enhancement in
Brazing & Soldering (forerunner of Soldering and Surface Mount Technology)
approx ten years ago. His hypothesis was that the conformal coat provided
mechanical support, but I suspect reduction of corrosion/oxidation must
also play a significant part, so the field service benefits might be even
higher than accelerated test results indicate.
David Whalley
Manufacturing Engineering Department
Loughborough University
Loughborough
Leics LE11 3TU
UK
Tel. +44(0)1509 222930
Fax. +44(0)1509 267725
[log in to unmask]
http://www.lboro.ac.uk/departments/en/research/mp/david_whalley/index.html
At 02:16 PM 4/20/98 +0100, you wrote:
> We have some work done by the IVF in Sweden on this subject, can
>anyone else give me any other references so that we can add them to our
>library? I have a specific customer that this enquiry is for, so any help
>is much appreciated.
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|