Can anyone describe to me how they would do such a PWB in terms of processing
order and PWB finish selection?
The application is RF and perhaps higher frequencies, which means that we may
use materials ranging from Arlon 25N, rogers 4003 all the way to the traditional
Rogers 6002..few layers...ratio of solderable pads to bondable is about 7 to 1
with about 100 pads on the whole board...1 by 1.5" in size...
Are immersion Au, electrolytic Au, fused solder or Hasl viable options?
thanks,
Marcelo
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|