Has anyone answered the original question?
for the record
7629 is about the same as 7628
fabric count warp yarn fill yarn wt thickness
(W-F) (oz/sq.yd) (inch)
====== ======= ========= ========= ======== ==========
7628 44 - 32 ECG75-1/0 ECG75-1/0 6.00 0.0068
7629 44 - 34 ECG75-1/0 ECG75-1/0 6.25 0.0070
I don't have the data on 2165 at home, if no one answers I'll send it tommorrow.
Dave Rooke
Viasystems Canada
Pointe Claire
= = = = =
>Hi all,
>
>for the PCB laminate FAQ I look for following details for prepreg types
>2165 + 7629:
>
>Type
>Weight [g/mē]
>Thickness [mm]
>Warp/Weft
>
>Please reply to us direct: [log in to unmask]
>
>Best regards
>
>jens Behrens
>
>The laminate FAQ: http://www.felsweb.com/lam_faq.htm
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
>For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
>################################################################
>
>
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################