It all comes down to cosmetics.
A nice shiny floor or a flat/dull floor?
The negative comments about waxes or ccoatings are related to durabiliy,
sensitivity to moisture and wear characteristics.
in your case, the waxing or coating would provide a shiny or gloss
finish.
Thereafter you could get away with a water buff (talk to a floor
cleaning source) and spot touchup without having to recoat (for
cosmetics) for a long long time.
The minimum would be a water buffing for removal of debris, dust and
marks on the surface.
Good Luck!
> -----Original Message-----
> From: SteveZeva [SMTP:[log in to unmask]]
> Sent: Tuesday, April 28, 1998 12:04 PM
> To: [log in to unmask]
> Subject: [TN] GEN:Conductive Floor Tile Care
>
> Good Day All!
>
> I've just joined a start-up company, and really we had a stroke
> of luck
> with the building we're moving into. Not only do I have most of the
> power,
> compressed air lines, and exhaust ducting I need for the equipment
> already
> routed and installed out on the production floor, but we also have
> conductive
> tile on the floor too! (...and that stuff not be cheap!)
>
> We're going to be a contract assembly company, I know that it
> always
> makes a good impression with potential customers to walk on to a
> manufacturing
> floor that is clean and shiny, and that's my problem...
>
> I searched the technet archives about esd floor care and
> conductive
> waxes, and there were a lot of negative comments when it came to esd
> waxes...many said they weren't dependable and could even cause
> problems...not
> to mention the cost, it's well over $25.00 a gallon and we've got a
> good
> 10-12,000 square foot manufacturing floor...
>
> ...Does anybody know of any good waxes?
> ...Any that don't cost an arm and a leg?
> ...Should I even wax the floor?
>
> I appreciate any comments!
>
> -Steve Gregory-
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
> 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC web site (http://jefry.ipc.org/forum.htm) for
> additional information.
> For the technical support contact Dmitriy Sklyar at [log in to unmask] or
> 847-509-9700 ext.311
> ################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|