PPM= defects found/possible defects X 1,000,000
Possible defects are all parts on the board, the board and all
terminations.
A misaligned component with off pad leads can be counted as a misaligned
component or as some number of leads off pad , but not both.
A missing soic8 can be a missing part or 8 open joints, but not both.
In order to use the PPM as a tool and as a metric of "goodness" of an
assembly, I prefer to assign the number of joints failing an acceptable
inspection and then use an unacceptable PPM rate as a prompt to analyze
the cause(s) of the unacceptable defect rate.
> -----Original Message-----
> From: [log in to unmask] [SMTP:[log in to unmask]]
> Sent: Tuesday, April 28, 1998 5:41 AM
> To: [log in to unmask]
> Subject: [TN] PPM calculations
>
> Dear colleagues
>
> We have some argues regarding PPM calculations, For an example: for
> placement station of automatic SMT components, do we have to count the
> soldering pads or only the components.
> If only the components its not the same level of difficult for
> capacitor
> and fine pitch.
> The same question is for dispensing machine of SMT glue.
> Please E Mail me the general formula for PPM calculation.
>
> Thanks and Best Regards
>
> Rokah Reuven
>
> IPC Member
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
> 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC web site (http://jefry.ipc.org/forum.htm) for
> additional information.
> For the technical support contact Dmitriy Sklyar at [log in to unmask] or
> 847-509-9700 ext.311
> ################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|