TECHNET Archives

April 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
X-To:
Date:
Fri, 24 Apr 1998 17:41:41 EDT
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Engelmaier <[log in to unmask]>
Content-type:
text/plain; charset=US-ASCII
Subject:
From:
Engelmaier <[log in to unmask]>
Content-transfer-encoding:
7bit
Parts/Attachments:
text/plain (27 lines)
Hi Ed,
Thermal shock is NOT an accelerated test for loading due to thermal cyling.
The damage mechanism is different then thermal cycling and therefore passing a
thermal shock test does not assure 10 years of life in thermal cycling.
Thermal shock can be used for ESS and for HAST testing to increase general
robustness.

Werner Engelmaier
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL  32174  USA
Phone: 904-437-8747, Fax: 904-437-8737
E-mail: [log in to unmask]

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################


ATOM RSS1 RSS2