ENID,
You may be able to clean and brush plate, depending upon the quantity. Another
thought is buss the fingers at the top (using wire, or possibly a conductive pen)
and replate gold over the nickel/gold. Be careful to prepare the surface properly,
no sense in trading your existing problem for a new one.
If you can obtain the connector specification, you may be able to determine if
the area in the bottom is used or not. If not, they may be salvageable as is (yuck,
I hated to say that). If all else fails, use a yellow magic marker(JUST KIDDING!!)
Are you the end user or the manufacturer? If you are the end user, your vendor owns
the problem. If you are the manufacturer, consider cleaning, bussing, and gold
plating the entire connector. How many panels and what percentage of the panel is
effected. AS important, has the issue been addressed? JOHN
[log in to unmask] wrote:
> Thanks for your prompt response. The real problem is not expose copper,
> but exposed nickel at the bottom edge of the finger that in some instances
> extend above 0.020" (refers to attached drawing).
>
> Any information is appreciated.
>
>
>
> ______________________________ Reply Separator _________________________________
> Subject: Re: [TN] Expose nickel in gold fingers
> Author: Non-HP-john01 ([log in to unmask]) at HP-PuertoRico,mimegw1
> Date: 4/22/98 6:01 PM
>
> Buenes Tardes Enid,
> A couple of questions first:
> 1) is the exposed copper from the bevel?. If so, No problemo!
> 2) Quantos Cobre y donde es ta? (pits, scratches, pinholes, etc)
> 3) is the exposed copper in the area where the contact mates with the connec
> tor?.
> If you want to Email me, I can discuss further an maybe we can solve. If you
> Email me, I will
> give you my phone number.. Jo hablo poquito Espanol y me Espanol es malo. Lo
> ciento, paro jo
> tratar muy deficil..
>
> [log in to unmask] wrote:
>
> > We are experiencing nickel exposure at the bottom edge of gold fingers.
> > What will be the risk of accepting it, if any? Is there any specification
> > about a maximum allowed???
> >
> > Enid Dávila
> >
> > ################################################################
> > TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> > ################################################################
> > To subscribe/unsubscribe, send a message to [log in to unmask] with following te
> xt in the body:
> > To subscribe: SUBSCRIBE TechNet <your full name>
> > To unsubscribe: SIGNOFF TechNet
> > ################################################################
> > Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional info
> rmation.
> > For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-
> 9700 ext.311
> > ################################################################
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text
> in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional inform
> ation.
> For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-97
> 00 ext.311
> ################################################################
>
> ------------------------------------------------------------------------
>
> Name: expnic~1.bmp
> expnic~1.bmp Type: Bitmap Image (image/bmp)
> Encoding: base64
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|