Srs.
You can see the IPC-SM-786-A standard (Dry pack ware) or if you speack
german... DIN TM3P49-005/01,
Boths are similars, and make reference to "Dry pack scale":
scale Description
1 Not sensitive
2 Sensitive limited
3 Sensitive
4 & 5 Very sensitive
6 Dry before use
Also has referencences about Bags (MIL.std-81075), desecants
(MIL-D-3463) and labels (IPC-788-005).
see you techneters.
Francisco Briceno
Molex de Mexico
______________________________ Reply Separator _________________________________
Subject: [TN] Storage conditions of pcb
Author: Ian Parker <[log in to unmask]> at INTERNET
Date: 4/21/98 5:10 PM
Good Day!
Could anyone advise me on the specification to adopt ( temperature and
relative humidity ) for the optimium storage conditions for bare printed
circuit boards.
These boards are typically overmakes which we store until our Customers
can place their next order.
What length of time do you think the solderability of solder levelled
boards would remain excellent in these conditions.
Best regards
Ian Parker
Prestwick Circuits
Scotland
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text
in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|