I have at previous employers.
Changing the nozzle (or gun) is required if the viscosity changes beyond
the limits of the nozzle.
Some spray systems are incompatable with some of the newer coatings.
Moisture sensitive materials should not use systems where moisture laden
air contacts the coating before it exits the gun (common on some types of
atomization systems).
A 33% solids coating requires .006 in of deposit for .002 of coating
thickness, while solventless material only needs app. 1 mm of coating. Some
nozzles cannot handle the lower flow rate.
Also, some suppliers do not totally understand the new coatings, yet.
In short, it depends upon the coating and the gun.
Aric Parr
-------------
Original Text
From: C=US/A=INTERNET/DDA=ID/TechNet(a)IPC.ORG, on 4/17/98 7:12 AM:
Hi Technetters
Can anyone provide information about experiences with new solventless
coatings on Selective Coating equipment.
Have you been obliged to change application heads or use special dispense
pressures? We are trying to help out some customers who are receiving
conflicting information and would appreciate any TechNetter input
Kindest regards
Graham Naisbitt - Concoat Ltd
Alasan House
Albany Park
Camberley, Surrey GU15 2PL UK
Tel: +44 (0) 1276 691100
Fax: +44 (0) 1276 691227
E-Mail: [log in to unmask]
Regards, Graham Naisbitt
Concoat Ltd
Alasan House, Albany Park
CAMBERLEY GU15 2PL
UK
Phone: +44 (0)1276 691100
Fax: +44 (0)1276 691227
email: [log in to unmask]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|