TECHNET Archives

April 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
X-To:
Date:
Tue, 14 Apr 1998 23:45:34 EDT
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, SteveZeva <[log in to unmask]>
Content-type:
text/plain; charset=US-ASCII
Subject:
From:
SteveZeva <[log in to unmask]>
Content-transfer-encoding:
7bit
Parts/Attachments:
text/plain (114 lines)
Dennis,

     I know this is different than what most everybody else is suggesting, but
whenever I've needed a means to manually print some boards, I've gone to this
company called The Ernst W. Dorn Company. They're into printing supplies and
equipment mainly for silkscreening type work...ya' know, T-shirts and stuff
like that. But that industry has a lot in common with us guys in electronics
when it comes to printing.

    They carry a very inexpensive manual printing table that has a precise
hinge that the stencil is mounted to (by the way, you can use ANY sized frame
you want to...), and a nice thick plexiglass plate where the PCB will be
located that has adjustment screws in the X and Y axis to adjust the
registration of the PCB to the stencil. You use double-sided sticky tape with
Carlson contact pins to locate the board beneath the stencil. It also has the
capability to adjust for snap-off (although if you're printing with a stencil
I don't why you would want snap-off).

     I've bought two of the tables for different companies that I've worked
for...everybody needs a simple manual printing table at one time or another to
do the "one'sies" and "two'sies" that seem to pop-up every now and again...ya'
know, prototypes...

     The table is called a Palomar Printing Table with Micro-adjust. The last
time I bought one, it was only around $1,500. Ernst W. Dorn also sells
squeegee material in a variety of shapes and durometers as well as sqeegee's
that are mounted in wooden handles for manual printing, you buy it by the
inch.

     They also carry a few other things that us guys in electronics find
useful, cheaper than you would find at someplace like Marshalls or Com-Kyl.
Like Peak Measuring Microscopes with reticles in the optics so you can measure
pad dimensions on PCB's, or stencil aperture dimensions (just to keep your
stencil vendor honest...hehehe).

     They have a WEB site, it's:  www.ewdorn.com   I've pasted the phone
numbers to their offices at the end of this post...

                                                                             H
ope this'll help ya' out!!


-Steve Gregory-

Equipment and Parts Warehouse:
Gardena (California)

Operation Manager: Helcio Trindade
333 West Alondra Avenue
Gardena, CA 90248
Phone: (310) 523-3676

(800) 992-3676
Fax (Equipment and Parts): (310) 523-3612

------------------------------------------------------------------------
Mid West Service Center:
Columbus (Ohio)

Service Director: Bobby Longendyke
Service Schedules, Parts, Installs and Technical Support

Phone: (800) 453-1982
Fax (Equipment and Parts): (614) 529-6621

------------------------------------------------------------------------
Branch Locations

NORTHERN CALIFORNIA

2951 Gordon Avenue
Santa Clara, CA 95051

Phone: (408) 245-3630
Fax: (408) 245-1314



DENVER AREA

2995 So. Tejon Street
Englewood, CO 80110

Phone: (303) 781-367
Fax: (303) 761-7913


SEATTLE AREA

7831 159th Place N.E.
Redmond, WA 98052
Phone: (425) 883-2674
Fax: (425) 881-5419


DALLAS AREA

5621-B East Rosedale
Forth Worth, TX 76112
Phone: (800) 637-3676
Fax: (817) 457-5598

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################


ATOM RSS1 RSS2