I am also in the beginning throes of paste in hole. But I will be
trying to dispense the paste. Are you planning on screening or
dispensing?
______________________________ Reply Separator _________________________________
Subject: [TN] paste-in-hole components
Author: [log in to unmask]> Jeff Hempton
<[log in to unmask] at internet
Date: 4/9/98 4:18 PM
Greetings fellow Technetters,
I am in the beginning throes of implementing serious paste-in-hole
(PIH) here at UT. I have some limited experience/success in this area,
but would like to tap into some of you PIH users that have been
involved longer, and are Grand Wizards of the PIH process:
1) Could you please forward any info you can share on component
suppliers that are manufacturing/willing-to-manufacture leaded
components (connectors,etc.) for this process?
2) Same question for feeder manufacturers, taping houses, etc.
If you are a vendor, please respond to me directly instead of
replying to Technet. ANY info shared would be DEEPLY appreciated.
Thanx in advance!
United Technology Electronic Controls
Jeff L. Hempton, Sr. SMD Engineer
3650 West 200 North
Huntington, In
46750-9002
Phone: 219-359-3514
Fax: 219-358-0695
E-mail: [log in to unmask]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text
in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|