No, I have not seen a good easy way to inspect BGA spheres. One thing that
compounds the inspection problem is the reflectivity of the solder spheres.
It becomes very difficult for a pick and place machine's vision system to
accurately define the edge of the sphere (i.e. a circle in 2-D). One method
to inspect is using oblique light and a low power microscope.
To answer the second part of your question: What should one look for?
a) Missing spheres
b) odd shaped spheres
c) large or small spheres
d) bridges
e) loose spheres
Thanks
Sundeep Nangalia
MCNC
e-mail:[log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of HGross1029
Sent: Thursday, April 09, 1998 2:47 PM
To: [log in to unmask]
Subject: [TN] BGA's
Is there a good and easy way to inspect BGA balls ?
Is there a piece of equip. available?
What should one look for ?
thanx...hg
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|