Dear Technet,
We'd like some clarification (interpretation) of the
requirements noted in:
J-Std-001B pg.27 paragraph 10.1.2.2 - Coating Coverage...
IPC-A-610B pg.74 paragraph 7.1.2 - Coating Coverage...
d. Be free of voids, BUBBLES, or foreign material which EXPOSE
component conductors, printed wiring conductors (including ground
planes) or other conductors, and/or violate design electrical spacing.
Does the word "expose" in (d.) above mean;
- No voids, bubbles, or foreign material "over" the runs (that the
bubbles may open over time due to temperature and pressure variations
and "expose" the conductors)?
- That voids, bubbles, or foreign materials indicate an absence of the
minimum required thickness of conformal coating?
- Or the literal meaning of "expose" - to leave bare, endanger?
We have received some PWAs with conformal coating that have
bubbles between and over conductor runs and around and on
components. The bubbles over the runs are not broken open (not
literally exposing the conductor). The coating when viewed
with the unaided eye appears hazy due to the multitude of tiny
bubbles throughout the coating. There are larger bubbles and
small bubbles between runs that when added together would
violate the minimum spacing requirements. As I mentioned
before, the bubbles are of various size and numerous enough to
make the coating appear porous (spongy looking) mostly tiny
bubbles throughout. We are required by contract to meet
J-Std-001B class 3.
We would appreciate your help in sorting through this confusion.
Thanks,
Dominick Scarano
Lockheed Martin
Mfg. Training
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|