Hi there,
When ablating polyimide structures, sometimes instead of getting a
clean finish you actually produce very small cone like structures in
the ablated section. This phenomena is due to particles of carbon
landing on the substrate and therefore acting as a mask.
Does anyone know of a method of replicating this onto a copper,
aluminium or gold substrate rather then the polymide substrate that i am currently aware of (i.e. what
material is required to act as the small particles for the mask, how would the particles be
applied and at what size, what laser fluence levels are required and
at what wavelength ?).
Thanks very much
Gareth Jones
Celestica Ltd
[log in to unmask]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|