Jim,
I can only speak for my own site, but we do solderability testing in three
cases:
1) Components that have never been used before
2) Components exhibiting solderability problems on the shop floor
3) Components with a manufacturing date older than eighteen months. This is
done when they come in/are used which are usually the same.
Hope this helps.
regards,
Bev Christian
Nortel
Belleville, Ontario
CANADA
> ----------
> From: Jim Marsico 516-595-5879[SMTP:[log in to unmask]]
> Sent: Thursday, March 26, 1998 2:34 PM
> To: [log in to unmask]
> Subject: [TN] ASSY: PARTS SOLDERABILITY
>
> I've been struggling with this question for a couple of years now, and it
> came
> up again...
>
> Can anyone share with me their component solderability policy? Are you
> performing solderability testing at incoming inspection for all parts?
> Are you
> testing for solderability again prior to assembly processes? Are you
> meeting
> J-STD-001 solderability requirements (para 5.2) and J-STD-001
> solderability
> maintenance requirements(para 5.4)? If so, how? Or are some of you
> claiming
> to meet J-STD-001 without doing any of the above?
>
> Any comments will be helpful.
>
> Thanks,
>
> Jim Marsico
> AIL Systems, Inc.
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
> information.
> For the technical support contact Dmitriy Sklyar at [log in to unmask] or
> 847-509-9700 ext.311
> ################################################################
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|