Hi,
What actually accounts for the large black patches on pads when the
technology goes wrong? Are these sulphates?
Regards
and it is quiet difficult to find somebody (except the
>supplier) who has production experience. I had some experience of work with
>electroplated silver coatings. The major problem of silver surfaces is
>tarnishing. The solderability of silver is good but significantly degrades
>when sulfides form on the surface. Under high temperature, the sulfides react
>with oxygen and form sulfates. One of the solutions to this problem is
>protection of silver with anti-tarnishing coatings (BTA, etc.). However, all
>these coatings are extremely fragile and can be easily destroyed. It was also
>observed that the thin coatings (thinner than 40 uin) degrade much faster.
>This problem was solved by placing an intermediate nickel layer.
>
>
>Chris
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
>For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
>################################################################
>
>
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|