What is being described here are: a minimum acceptable condition;, a max
recommended (process indicator type info) and max allowable (ie. not
acceptable) condition
Min Acceptable: the lead shall be discernible in the
completed solder
connection (NOTE: SHALL describes condition
which is a requirement for Class 3 and Class 2
(where no process control plan exists) but is only
recommendation for Class 2 (with process control plan) and Class 1)
Max Recc (Indicator): The lead should not extend more
than 1.5 mm (measured
vertically) from the PWB surface
Max Acceptable: the lead must not violate minimum
electrical spacing requirements
(NOTE: MUST denotes condition
rejectable for all classes.)
> ----------
> From: Letteri, Maryanne E
> (FL51)[SMTP:[log in to unmask]]
> Reply To: TechNet E-Mail Forum.;Letteri, Maryanne E (FL51)
> Sent: Thursday, March 19, 1998 10:50 AM
> To: [log in to unmask]
> Subject: [TN] J-STD-001B Question
> Importance: High
>
> Please answer the following concerns:
>
> J-STD-001B Para 6.5.3 2nd paragraph:
>
> As a min., the lead shall be discernible in the completed solder
> connection. The lead should not extend more than 1.5 mm (measured
> vertically) from the PWB surface and the lead must not violate minimum
> electrical spacing requirements.
>
>
>
> The questions is:
> Can we have both ways or is there just one way for this process?
>
> Must the leads be discernible or do we have to have the lead extend
> throughout the board.
>
>
>
> Maryanne Letteri
> Quality Specialist
>
> PS. Lee Gilgosch who works with me is a member of IPC.
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
> 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC web site (http://jefry.ipc.org/forum.htm) for
> additional information.
> For the technical support contact Dmitriy Sklyar at [log in to unmask] or
> 847-509-9700 ext.311
> ################################################################
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|