Edward Szpruch wrote:
>We are considering cleaning of innerlayers by adhesive rollers just before
>lay-up . We are applying reduced black oxide , 0.4 mg/sqcm . AOI is done
>before black oxide .
>We allready made preliminary test and we had no problems with delaminations
>etc . My questions are :
>1 ) Does anyone performing similar kind of cleaning after black oxide ?
>2 ) What kind of negative effects should be exepcted ? ....

Edward

We use adhesive rollers before lay-up but never after black oxide.
The surface is clean after black oxide so it's not necessary to clean it again.
We have also tested it and we had problems with delamination.

Best regards

Simon

------------------------------------------------------------------------------------
Optiprint AG
Simon Huetter           Tel.:   +41 71 878 77 77
Dipl. El. Ing. HTL      Fax.:   +41 71 878 77 66
R&D                     e-mail:  [log in to unmask]
------------------------------------------------------------------------------------
http://www.optiprint.ch
------------------------------------------------------------------------------------

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################


ATOM RSS1 RSS2