Lee McCuistion wrote:
>
> Ok,
> Who has some technical details, study, or white paper on the validity
> of, or problems with mating tinned fingered SIMMs with gold contact
> sockets or visa-versa? Does this really have any effect on
> reliability?
>
> Lee McCuistion
> Manufacturing Engineer
> Cubix Corporation
> 2800 Lockheed Way
> Carson City, NV 89706
> 702-888-1000 x237 (voice)
> 702-888-1002 (fax)
> [log in to unmask] (e-mail)
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
> For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
> ################################################################
There is plenty of literature on this subject. DO NOT MIX GOLD PLATED
CONTACTS WITH TIN PLATED CONTACT. It is a serious reliability problem.
For details see pages 250-251 in " Failure Modes and Mechanisms in
Electronics Packages" Published by Chapmann & Hall.
To order contact:
International Thomson Publishing
7625 Empire Drive, Florence, KY 41042
Tel. 1-800-842-3636
email: [log in to unmask]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|