Dear Ed,
We had the same problem sometime back in 1997 and it gave us
nightmare. We need to clean the bags and remove all the crystals
formed on the anode baskets once in two week. Are you doing that!!!
How we solved it?
Check your copper sulphate's concentration and bring it to the minimum
level. We did that and until todate no more crystallisation
Estee, April 01 '98.
______________________________ Reply Separator _________________________________
Subject: [TN] Copper sulfate crystals
Author: ,"TechNet E-Mail Forum." <[log in to unmask]>, at internet
Date: 3/30/98 10:52 PM
Has anyone ever experienced a problem of copper sulfate crystals =
developing on the bottom of anodes inside the anode bags? If so, what =
causes it and how do you get rid of it.=20
thanks,
Ed Cosper=20
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text
in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|