We just had a couple of PWB types built incorrectly due to bad electronic
data being sent to our board houses. Unfortunately we did not catch either
problem until we had fully assembled the boards.
Problem A was due to the wrong aperture file being sent out resulting in no
power plane connections. Problem B was due to an old design tool which
did not show a "filled in" power plane which was required. No netlist data
was available for either design.
We would like to continue with an all electronic process but need some
fool-proof checks that will detect if we send some incorrect file(s)/data
or our board house does something wrong. I'm sure companies are doing this
sucessfully all the time (and all electronic). How are people making this
process work well for them?
---
Gregg Klawson
GTE Government Systems Corp, Taunton, Massachusetts, USA
[log in to unmask], telephone +1.508.880.1822
The views expressed are the author's and do not necessarily reflect the
official position of GTE or any of its subsidiaries.
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|