TECHNET Archives

March 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Jack Crawford <[log in to unmask]>
Date:
Wed, 18 Mar 1998 11:30:57 -0600
Content-Type:
text/plain
X-To:
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Jack Crawford <[log in to unmask]>
Parts/Attachments:
text/plain (143 lines)
Great Question!
IPC sponsors additional FREE technical forums run on our LISTSERV system.  Full
descriptions are available from our web site http://www.ipc.org  Scroll down to the
IPC On-Line Services icon on the left side and that will take you to the right place.
 Abbreviated info follows:

TechNet: used to ask others for technical help, comments or questions on IPC
specifications, or other technical inquiries.

Designer Council: means to stay current with the many programs of the IPC Designers
Council, and to exchange information with other designers.

ComplianceNet: covers environmental, safety and related regulations or issues,
regulatory proposals, alerts and draft comments, legislative updates, new regulatory
interpretations (i.e., photo resist skins), Grass roots action alerts, compliance
assistance

IPCsm840: very specific; comment, help or get help on issues relating to
"Qualification and Performance Specification of Permanent Polymer Coating
(Soldermask) for Printed Boards."

ChipNet:  very specific, comment, help or get help on issues relating to
ANSI/J-STD-012, "Implementation of Flip Chip and Chip Scale Technology."

Roadmap:  very specific, provides opportunity for information exchange that
facilitates coordinated development of IPC's National Technology Roadmap for
Electronic Interconnections.

IPC_New_Releases:  Provides notification to subscribers when new and revised IPC
publications are available.

GenCAM:  used for comments or questions on IPC's effort to standardize electronic
data transfer strategies (DTS) and other inquiries regarding transferring files from
CAD to CAM. IPC will also use GenCAM to announce meetings, important technical
issues, new developments, etc.


Jack Crawford, IPC Project Manger - Assembly
2215 Sanders Road, Northbrook IL  60062-6135
[log in to unmask]        http://www.ipc.org
847-509-9700 x 393
fax 847-509-9798

>>> Paul Terranova <[log in to unmask]> 03/18/98 09:10AM >>>
Jan,

Is there really a Chipnet? How can those of us interested subscribe to
this forum? I've been looking for other forums similar to Technet
related to the microelectronics industry. If anyone else has any other
good recommendations, please let me know.  Thanks.

Paul Terranova
Analytical and Environmental Test Services Lab
Worldwide Module Components Group

 Digital Equipment Corp
 200 Forest Street
 Mail Stop: MRO3-1/D2
 Marlboro,  MA  01752-3085

'    Phone: (508)467-3109
* Fax: (508)467-6796
* Email: [log in to unmask]

        -----Original Message-----
        From:   Jan Vercammen [SMTP:[log in to unmask]]
        Sent:   Monday, March 16, 1998 9:16 AM
        To:     [log in to unmask]
        Subject:        [TN] leadframe materials

        hello,

        I have a few questions concerning package leadframe materials of
integrated
        circuit packages. I have subscrided only recently to ChipNet and
I will
        submit the same questions there. However, some of the
subscribers on TechNet
        may have valuable info on the subject.

        -1- are non-copper materials (e.g.Invar, Kovar or Alloy-42 which
are Fe-Ni
            alloys) still used alot for leadframe design of surface
mount devices?
            What is the percentage of copper leadframes on the market
today?
        -2- is there a finish used for copper leadframes and, if so,
what materials
            are used and what is the covered thickness?
        -3- who has information on or can list references or literature
on the complex
            permeability of non-copper leadframe materials ( (e.g.Invar,
Kovar or
            Alloy-42)

        All help, however small is appreciated.


        regards,

        Jan Vercammen

        ################################################################
        TechNet E-Mail Forum provided as a free service by IPC using
LISTSERV 1.8c
        ################################################################
        To subscribe/unsubscribe, send a message to [log in to unmask]
with following text in the body:
        To subscribe:   SUBSCRIBE TechNet <your full name>
        To unsubscribe:   SIGNOFF TechNet
        ################################################################
        Please visit IPC web site (http://jefry.ipc.org/forum.htm) for
additional information.
        For the technical support contact Dmitriy Sklyar at
[log in to unmask] or 847-509-9700 ext.311
        ################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700
ext.311
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################


ATOM RSS1 RSS2