Kathy,
Try the following persons at Enthone OMI (West Heaven CT).
They have the answers your're looking at...
Bob Farrell
Eric Strafstrom
Durand Cerone
Good luck.
Michel Poulin
Technical advisor / Conseiller Technique
V I A S Y S T E M S CANADA.
379 Brignon Granby, Quebec (Canada) J2G 8N5
Tel.: ( 514 ) 378-0193, FAX: ( 514 ) 378-5110
E-MAIL: [log in to unmask]
> ----------
> From: Kathy Palumbo[SMTP:[log in to unmask]]
> Reply To: TechNet E-Mail Forum.;Kathy Palumbo
> Sent: Friday, March 13, 1998 5:00 PM
> To: [log in to unmask]
> Subject: [TN] OSP COATED BOARDS
>
> We are in the process of performing an analysis on OSP coated boards
> as
> an alternative to HASL coated boards. So far everything looks
> excellent. Outstanding wetting, solderability, less solder bridging
> issues, better paste printing results, better component placement
> results, better match of pad geometry with gerber data, no bow and
> twist
> problems, flatter board surface, etc., etc.....
>
> However our Manufacturing manager is concerned with the following
> issues:
>
> 1. Moisture Sensitivity
> 2. Scratches through the OSP coating
> 3. Finger print sensitivity
> 4. Stricter Handling requirements
>
> Will the boards have to be vacuumed sealed with desiccant to prevent
> moisture damage? How sensitive are the boards to finger prints? What
> is the typical shelf life of an OSP coated board? If the boards are
> scratched through the OSP coating will we have soldering problems
> later?
>
>
> Is there a contact person at Enthone (our supplier used ENTEK OSP
> coating) who could help me with some of this?
>
> These are just a few questions that need to be addressed, and any
> response regarding this matter will be greatly appreciated.
>
>
> Thanks in advance for your help!
>
> Kathy Palumbo
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
> 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC web site (http://jefry.ipc.org/forum.htm) for
> additional information.
> For the technical support contact Dmitriy Sklyar at [log in to unmask] or
> 847-509-9700 ext.311
> ################################################################
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|