I am currently looking at this coating as an alternative to HASL for our
product. I have looked at all of the other alternatives and was not
satisfied with the results for our product (memory boards). I believe
that alternative coatings should be looked at on a case by case basis.
What works for me might not work for you.
I set up my own experiment for several different products which we build
to see if the alternative coatings would be acceptable for our processes
and our product. I am still in the process of analyzing the alphalevel
boards (waiting on samples). I was told these alphalevel boards can be
treated just like a HASL coated board and do not require any type of
special handling. This characteristic is important for us here at
Viking.
I think the best approach for you would be to perform your own analyses
on your product as well. You could also give Steve Beagle with Alpha a
call at (219) 922-7990. He has been doing a similar analyses with this
product for the past two years and has literally soldered thousands of
boards. I think he can answer any technical questions you might have
regarding the alphalevel product.
Good Luck!!
Thanks,
Kathy Palumbo
> ----------
> From: Rob Emery[SMTP:[log in to unmask]]
> Sent: Tuesday, March 24, 1998 7:16 AM
> To: [log in to unmask]
> Subject: [TN] AlphaLevel as replacement for Electroplated Nickel
> Gold
>
> We've recently had some problems with flaking of gold plate on keypad
> fingers on a pcb.
>
> Consequently, we're considering changing the finish to AlphaLevel,
> although we've been unable to find any major examples of companies who
> are using AlphaLevel 'unsoldered' in this type of application.
>
> Does anyone have any experience of the long term problems we might
> encounter if we make this change, eg degradation of contact causing
> erratic keypress operation?
>
> Regards
>
> Rob
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|