The min resistivity value for Si wafers is 12 .
ashok
> ----------
> From: Mike Masters[SMTP:[log in to unmask]]
> Sent: March 9, 1998 9:06 AM
> To: [log in to unmask]
> Subject: Re: [TN] Wafter Diceing Water Req.
>
> Hi David,
>
> I can't tell you the actual specifications, but we use 17 Meg. DI for
> dicing operations. I have
> seen it drop to as low as 15 Meg. DI. This is wafer on the expand
> sheet.
>
> Hope this helps,
>
> Mike
>
> David D Hillman wrote:
>
> > Hi TechNet - I am looking for info/opinions/etc. to the following
> question:
> >
> > What level of resistivity (e.g. 2 Megohm,or 18 Megohm) of water do
> you
> > suggest using or have had success using for wafer sawing operations
> for
> > both silicon and GaAs materials?
> >
> > Dave Hillman
> > Rockwell Collins
> > [log in to unmask]
> >
> > ################################################################
> > TechNet E-Mail Forum provided as a free service by IPC using
> LISTSERV 1.8c
> > ################################################################
> > To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> > To subscribe: SUBSCRIBE TechNet <your full name>
> > To unsubscribe: SIGNOFF TechNet
> > ################################################################
> > Please visit IPC web site (http://jefry.ipc.org/forum.htm) for
> additional information.
> > For the technical support contact Dmitriy Sklyar at [log in to unmask]
> or 847-509-9700 ext.311
> > ################################################################
>
>
>
> --
> /\
> _\/_
> /_/\_\
>
> Mike Masters
> QA Materials Engineering Section
> Office: (919) 479-3771
> FAX: (919) 479-3328
> Internet: [log in to unmask]
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
> 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC web site (http://jefry.ipc.org/forum.htm) for
> additional information.
> For the technical support contact Dmitriy Sklyar at [log in to unmask] or
> 847-509-9700 ext.311
> ################################################################
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|