Marletta,
It is preferred to have oblong lands to assist in concentrating the solder fillet
around the component lead. The IPC-SM-782 indicates oblong as optional but should
read preferred.
Regards,
Gary Ferrari
Executive Director
IPC Designers Council
(860) 350-9300 Fax (860) 350-9309
[log in to unmask]
>>> Marletta Tucker <[log in to unmask]> 03/31/98 03:13PM >>>
What is the deciding factor on whether or not an SMD parts land is squared off
or oblong? Could/should all SMD parts have oblong lands?
@ @ @ Thanks,
@ @ @ ///
@ * Marletta Tucker
@ @ > 1921 Hurd Dr. M/S 2-21
@@|\ _ Irving, Tx. 75038
@ | 972-518-7619
# [log in to unmask]
We have enough youth, how about a fountain of SMART?
The above views are my own, and do not represent those
of Abbott Laboratories.
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700
ext.311
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|