Good day ya'll!!
In light of all the discussion about Palladium, I went out "surfing" on
the NET to try and find something (anything actually) that would bear out the
concerns that some of us seem to have with Palladium platings.
I did this not to come up with references that I can throw back at people
who have a different opinion than my own, but to truely try and learn
something. I'm thinking; "Maybe I could be wrong about this after all, let's
try and find out if I am..."
As much as I could search over lunchtime, I couldn't find one site that
had any negative things to document as far as soldering and palladium as a
metal finish is concerned. That's not to say that there isn't some information
out there, but I couldn't find it on the WEB during lunch. I also went to
WWW.TI.COM, and typed "palladium" in their search engine at their site...It
came back with 11-hits of articles and papers that were out for anybody and
everybody to read regarding soldering to palladium.
So I'm really trying to keep a open mind about this, but it's getting
harder to do when I can't really find evidence of anything other than the
different solder joint apperance that occurs with a palladium coated lead.
If there really is some concern with the reliabilty of palladium, I
sincerely would like to know about it. After all, I figure I got at least
another 20-years of work in me till I can retire (unless I get lucky and win
the lotto...HA!), and I don't think I'm going to be changing feilds anytime
soon, so I'm going to have to deal with this for at least the next 20-years...
I'm not pretending to know all there is about palladium, because I know I
don't. I have run across a few other engineers that are just as passionate
about their positions on palladium plating and Texas Instruments as Ed is,
they hate them both...and I honestly don't understand why.
Can somebody please enlighten
me?
-Steve Gregory-
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|