Mr. Brucker,
I'd attach your TechNet reply, but errantly zapped it this morning
while scanning the Net. I did read it though, and you bring up good
points about inspection criteria. We routinely perform a physical
destructive analysis (DPA) of production boards, and I have cross
sectioned many of these joints. My own experience is that they've been
troublefree, and certainly achieve compliant heel and side fillets.
Toe fillets are not a requirement for gullwing leads because the
common presence of exposed copper from the shearing process, and
occasionally the permissible toe overhang, can make those fillets very
difficult to achieve. I see a request on the Net for info on palladium
finished boards; I've not run into them yet. That could be a blessing.
Bruce Tostevin
Benchmark Electronics
Hudson, NH
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|